Wednesday, 9 March 2016

Full Annealing

          If it is desired to reline the grain structure and produce a lamellar pearlite, a full annealing cycle should be used. This consists of heating the steel to a temperature above the transformation range, holding for one or two hours, and then cooling at a predetermined rate to obtain the desired microstructure. Grain refinement is accomplished in this instance by the re-crystallisation of the steel in passing through the critical range both in heating and in cooling. The microstructure obtained in cooling any steel from above the critical temperature range is dependent both upon the temperature range in that ranges. Thus, it is obvious that the rate at which any steel is cooled determines the final microstructure, since the degree of transformation will depend on the amount of time allowed for it to occur. Therefore, the slower the rate of cooling and the higher the temperature at which complete transformation occurs during full annealing, the coarse the pearlite will be with correspondingly lower hardness.
          Such treatment is performed usually on steel of 0.3 to 0.6 % carbon content which is to be machined.

Isothermal annealing

          It is a type of full annealing in which the steel first is cooled to the temperature at which it is desired to have transformation occurs, at a rate sufficiently rapid to prevent any structural change above that temperature. The steel then is held at the selected temperature for the time necessary to complete such transformation. Thus it possible, with this process to obtain a more uniform micro-structure that could be expected by continuous cooling. However, since it is necessary to drop the temperature rapidly to prevent any transformation above the desired temperature, there are definite limitations as to the mass that can be co-treated. It is applicable, therefore, only to small sections and would be suitable for large bars or large load in batch type furnace since in would be impossible to cool them at a rate sufficiently rapid to prevent some transformation.
          Isothermal annealing process not only improves machinability in general, but also results in a better finish by machining. However, it has the following important limitations:
          It is suitable only for small components. Heavy components cannot be subjected to this treatment because it is not possible to cool them rapidly and uniformly to the holding temperature at which transformation occurs. 

Tuesday, 8 March 2016

Process or Sub critical annealing

          Another type annealing called Process or Sub critical annealing consists of heating the steel to a temperature first under lower critical point and holding at this temperature for the proper time (2-4 hrs) followed by air cooling. This type of annealing results in softening the steel due to particle coagulation of the carbide to form the spheroids or small globules of carbide. It is not suitable when a close control of hardness or structure is desired, because the prior structure of steel determined to a marked degree the extent of spheroidisation which will occur.
          This process is quite satisfactory for rendering bars more suitable for cold sawing or shearing and is used to great extent for these purposes. Since the temperature to which the bars are heated is somewhat lower than in full annealing there is less scaling and warping can be controlled.   

Spheroidisation annealing

          It is a type of annealing which causes practically all carbides in the steel to agglomerate in the form of small globules or spheroids. There may be wide range of hardness with such a structure for any grade of steel since the size of the globules has a direct relation to hardness. Spheroidising may be accomplished by heating to a temperature just below the lower critical and holding for sufficient period of time. A more desirable and commonly used method for spheroidising is to heat to temperature just above the critical and cool very slowly (6°C per hour) through the critical range or to heat to a temperature within the critical range but not above the upper critical and cool slowly.
          This treatment is used for practically all steels containing over 0.6 percent carbon that are to be machined or cold formed.  

Saturday, 5 March 2016

Distinction between Annealing and Normalising

ANNEALING

NORMALISING
Main purpose of annealing is to 
relieve internal stresses
Main purpose of normalising is to 
improve mechanical properties.

Less hardness, more T.S & Toughness
Slightly more hardness, less T.S & Toughness.
Pearlite is coarse
Pearlite is fine and usually appears 
unresolved with optical microscope.
Grain size distribution is more.
Grain size distribution is less.
Internal stresses are least.
Internal stresses are slightly more.
Furnace cooling is employed.
Air cooling is employed.
Cooling rate is slow.
Cooling rate is high.
Costly and inconvenient.
Economical and more convenient.